A Six Sigma Methodology for Reducing Casting Defects in Foundry Operations

Six Sigma is an organized and systematic method for strategic process improvement that relies upon statistical & scientific methods to make reductions in defect rates. A case study is carried out in casting industry, where Six Sigma tools i.e. Taguchi approach for the defect reduction is implemented...

The International Journal of Technology, Knowledge, and Society

Common Ground Research Networks